Name Specific Heat Capacity Thermal Conductivity Melting Point Resource Effects
Copper Ore 0.386 4.500 1083.9°C Decor: +10%
Electrum 0.150 2.000 1063.9°C Thermally Reactive
Gold Amalgam 0.150 2.000 1063.9°C Decor: +10%

Overheat Temperature: +50°C Thermally Reactive

Iron Ore 0.449 4.000 1534.9°C None
Mercury 0.140 8.300 −38.8°C Thermally Reactive
Niobium 0.265 54.000 2476.9°C Decor: +50%

Overheat Temperature: +500°C High Thermal Conductivity

Pyrite 0.386 4.500 1083.9°C None
Steel 0.490 54.000 2426.9°C Overheat Temperature: +200°C

High Thermal Conductivity

Thermium 0.622 220.000 2676.9°C Overheat Temperature: +900°C

High Thermal Conductivity

Wolframite 0.134 15.000 2926.9°C High Thermal Conductivity

Thermally Reactive